Effect of silica coating combined to a MDP-based primer on the resin bond to Y-TZP ceramic

dc.contributor.authorMay, Liliana Gressler
dc.contributor.authorPassos, Sheila Pestana
dc.contributor.authorCapelli, Diana Barca
dc.contributor.authorOezcan, Mutlu
dc.contributor.authorBottino, Marco Antonio [UNESP]
dc.contributor.authorValandro, Luiz Felipe
dc.contributor.institutionUniversidade Federal de Santa Maria (UFSM)
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.contributor.institutionClin Fixed & Removable Prosthodont & Dent Mat Sci
dc.date.accessioned2014-05-20T14:05:22Z
dc.date.available2014-05-20T14:05:22Z
dc.date.issued2010-10-01
dc.description.abstractThe aim of this study was to evaluate the influence of silica coating and 10-methacryloyloxydecyl dihydrogen phosphate (MDP)-based primer applications upon the bonding durability of a MDP-based resin cement to a yttrium stabilized tetragonal zirconia (Y-TZP) ceramic. Ninety-six Y-TZP tabs were embedded in an acrylic resin (free surface for adhesion: 5 x 5 mm(2)), ground finished and randomly divided into four groups (N = 24) according to the ceramic surface conditioning: (1) cleaning with isopropanol (ALC); (2) ALC + phosphoric acid etching + MDP-based primer application (MDP-primer); (3) silica coating + 3-methacryloyloxypropyl trimethoxysilane (MPS)-based coupling agent application (SiO(2) + MPS-Sil); and (4) SiO(2) + MDP-primer. The MDP-based resin cement was applied on the treated surface using a cylindrical mold (diameter=3 mm). Half of the specimens from each surface conditioning were stored in distilled water (37 C, 24 h) before testing. Another half of the specimens were stored (90 days) and thermo-cycled (12,000x) during this period (90d/TC) before testing. A shear bond strength (SBS) test was performed at a crosshead speed of 0.5 mm/min. Two factors composed the experimental design: ceramic conditioning strategy (in four levels) and storage condition (in two levels), totaling eight groups. After 90d/TC (Tukey; p < 0.05), SiO(2) + MDP-primer (24.40 MPa) promoted the highest SBS. The ALC and MDP-primer groups debonded spontaneously during 90d/TC. Bonding values were higher and more stable in the SiO2 groups. The use of MDP-primer after silica coating increased the bond strength. (C) 2010 Wiley Periodicals, Inc. J Biomed Mater Res Part 8: Appl Biomater 95B: 69-74, 2010.en
dc.description.affiliationUniversidade Federal de Santa Maria (UFSM), Dept Restorat Dent, Div Prosthodont, BR-97119900 Santa Maria, RS, Brazil
dc.description.affiliationSão Paulo State Univ UNESP, Sao Jose dos Campos Dent Sch, Dept Restorat Dent, Sao Jose Dos Campos, SP, Brazil
dc.description.affiliationClin Fixed & Removable Prosthodont & Dent Mat Sci, Ctr Dent & Oral Med, Zurich, Switzerland
dc.description.affiliationUnespSão Paulo State Univ UNESP, Sao Jose dos Campos Dent Sch, Dept Restorat Dent, Sao Jose Dos Campos, SP, Brazil
dc.format.extent69-74
dc.identifierhttp://dx.doi.org/10.1002/jbm.b.31684
dc.identifier.citationJournal of Biomedical Materials Research Part B-applied Biomaterials. Hoboken: Wiley-liss, v. 95B, n. 1, p. 69-74, 2010.
dc.identifier.doi10.1002/jbm.b.31684
dc.identifier.issn1552-4973
dc.identifier.lattes9234456003563666
dc.identifier.urihttp://hdl.handle.net/11449/22936
dc.identifier.wosWOS:000281655900009
dc.language.isoeng
dc.publisherWiley-liss
dc.relation.ispartofJournal of Biomedical Materials Research Part B: Applied Biomaterials
dc.relation.ispartofjcr3.373
dc.relation.ispartofsjr0,715
dc.rights.accessRightsAcesso restrito
dc.sourceWeb of Science
dc.subjecttribochemical treatmenten
dc.subjectcoupling agentsen
dc.subjectbondingen
dc.subjectadhesionen
dc.subjectresin cementen
dc.subjectY-TZPen
dc.titleEffect of silica coating combined to a MDP-based primer on the resin bond to Y-TZP ceramicen
dc.typeArtigo
dcterms.licensehttp://olabout.wiley.com/WileyCDA/Section/id-406071.html
dcterms.rightsHolderWiley-liss
unesp.author.lattes9234456003563666
unesp.campusUniversidade Estadual Paulista (Unesp), Instituto de Ciência e Tecnologia, São José dos Campospt

Arquivos

Licença do Pacote
Agora exibindo 1 - 2 de 2
Nenhuma Miniatura disponível
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição:
Nenhuma Miniatura disponível
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: