Effect of antioxidant agents on bond strength of composite to bleached enamel with 38% hydrogen peroxide

Carregando...
Imagem de Miniatura

Data

2011-01-01

Orientador

Coorientador

Pós-graduação

Curso de graduação

Título da Revista

ISSN da Revista

Título de Volume

Editor

ABM, ABC, ABPol

Tipo

Artigo

Direito de acesso

Acesso abertoAcesso Aberto

Resumo

This study evaluated the effect of antioxidant agents on microtensile bond strengths (mTBS) of composite to bleached enamel. Fifteen freshly extracted human third molars were selected and randomly assigned to 6 groups (n = 5): (NB) enamel not bleached, (B) bleached enamel, (BR7) bleached enamel and restored 7 days later, (BSA) bleached enamel+sodium ascorbate, (BMC) bleached enamel+malvidin chloride, (BPC) bleached enamel+pelargonidin chloride. The groups were bleached with 38% hydrogen peroxide (HP - Opalescence Xtra Boost) and restored with Single Bond+Filtek Z350. The specimens were thermocycled and submitted to a microtensile load at 1 mm/min crosshead speed. The data were evaluated by ANOVA and Tukey test at 5% of significance. The mean and standard-deviation for all groups were: NB: 30.95(±11.97)a; BSA: 30.34(±8.73)a, BPC: 22.81(6.00)b, BR7: 21.41(±6.12)b, B: 14.10(±4.45)c, BMC: 13.25(±6.02)c. Sodium ascorbate reversed the bond strengths to enamel immediately after bleaching.

Descrição

Idioma

Inglês

Como citar

Materials Research. ABM, ABC, ABPol, v. 14, n. 2, p. 235-238, 2011.

Itens relacionados

Unidades

Departamentos

Cursos de graduação

Programas de pós-graduação