Jassé, Fernanda FerreiraCampos, Edson Alves de [UNESP]Lefever, DorienDi Bella, EnricoSalomon, Jean PierreKrejci, IvoArdu, Stefano2014-05-272014-05-272013-09-13Journal of Dentistry.0300-5712http://hdl.handle.net/11449/76554Objectives: This study evaluated the gloss behaviour of experimental resin composites loaded with different filler percentages, immediately after polishing and after toothbrushing simulation. Methods: Sixteen disc-shaped specimens were fabricated for each different-charged composite (40%, 50%, 60%, 70% and 75%) and polished with SiC abrasive papers. Gloss measurements were made prior to simulated toothbrushing. The specimens were subjected to the simulation for 5, 15, 30 and 60 min using an electrical toothbrush with a standardized pressure while being immersed in a toothpaste/artificial saliva slurry. Results: Baseline composite gloss values ranged from 69.7 (40%) to 81.3 (75%) GU (gloss units) and from 18.1 (40%) to 32.3 (75%) GU after 1 h of brushing. Highest gloss values were obtained by 75%-charged resin, while the lowest values were obtained by the 40%-charged one. Conclusions: All tested materials showed a gloss decrease. However, the higher filler load a composite resin has, the higher gloss it can achieve. Clinical significance: Gloss of resin composite materials is an important factor in determining aesthetic success of anterior restorations, and this property may vary according to the filler charge of the restorative material. Higher filler load of a composite resin results in higher gloss values. © 2013 Elsevier Ltd. All rights reserved.engComposite resinsDental polishingGlossToothbrushingInfluence of filler charge on gloss of composite materials before and after in vitro toothbrushingArtigo10.1016/j.jdent.2013.04.011Acesso restrito2-s2.0-848836358294566192900068248