Dias, D. S. [UNESP]Crespi, Marisa Spirandeli [UNESP]Kobelnik, M. [UNESP]Ribeiro, Clovis Augusto [UNESP]2014-05-202014-05-202009-08-01Journal of Thermal Analysis and Calorimetry. Dordrecht: Springer, v. 97, n. 2, p. 581-584, 2009.1388-6150http://hdl.handle.net/11449/41742PHB [poly (3-hydroxybutyrate)], post-consumer soft-drink bottles poly (ethylene terephthalate) PET (herein named PET-R) and PHBPET-R (blends of PHB and PET-R in several compositions) samples were evaluated by differential scanning calorimetry (DSC) and scanning electronic microscopy (SEM) in order to verify their thermal properties and porosity according to amounts of PET-R added the blends. The DSC curve showed that the solvents used to solve the polymer mixture cause changes in the thermal behavior of PET-R films and in PHBPET-R blends. SEM studies of the PHBPET-R blends show that with a gradual mass increase of PET-R, there are gradual increases in the porosity of the films.581-584engPolymerBiodegradationPolymeric blendPHBPETCalorimetric and SEM studies of PHB-PET polymeric blendsArtigo10.1007/s10973-009-0328-5WOS:000271108200035Acesso restrito747131011399914084983108918100820000-0002-7984-5908