Characteristics of the Cu-18.84 at.%Al-10.28 at.%Mn-1.57 at.%Ag alloy after slow cooling from high temperatures

dc.contributor.authorSilva, R. A.G.
dc.contributor.authorPaganotti, A.
dc.contributor.authorAdorno, A. T. [UNESP]
dc.contributor.authorSantos, C. M.A. [UNESP]
dc.contributor.authorCarvalho, T. M. [UNESP]
dc.contributor.institutionUniversidade Federal de São Paulo (UNIFESP)
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2018-12-11T16:58:05Z
dc.date.available2018-12-11T16:58:05Z
dc.date.issued2015-09-17
dc.description.abstractThe characteristics of the Cu-18.84 at.%Al-10.28 at.%Mn-1.57 at.%Ag alloy after slow cooling from high temperatures were studied using optical and scanning electron microscopies, microhardness measurements with temperature, differential scanning calorimetry, X-ray diffraction, magnetic moment changes with temperature and applied field. The results indicated the presence of a new transition associated with dissolution of the Ag-rich phase. It was also verified that the content of Al strongly interferes with the magnetization of the Cu-18.84 at.%Al-10.28 at.%Mn-1.57 at.%Ag alloy, since at lower Al concentration the relative fraction of the ferromagnetic L2<inf>1</inf>-(Cu<inf>2</inf>AlMn) phase is decreased.en
dc.description.affiliationDepartamento de Ciências Exatas e da Terra, UNIFESP
dc.description.affiliationDepartamento de Físico-Química, IQ-UNESP
dc.description.affiliationUnespDepartamento de Físico-Química, IQ-UNESP
dc.format.extent1233-1238
dc.identifierhttp://dx.doi.org/10.1007/s10973-015-4654-5
dc.identifier.citationJournal of Thermal Analysis and Calorimetry, v. 121, n. 3, p. 1233-1238, 2015.
dc.identifier.doi10.1007/s10973-015-4654-5
dc.identifier.issn1388-6150
dc.identifier.scopus2-s2.0-84939464072
dc.identifier.urihttp://hdl.handle.net/11449/171996
dc.language.isoeng
dc.relation.ispartofJournal of Thermal Analysis and Calorimetry
dc.relation.ispartofsjr0,587
dc.rights.accessRightsAcesso abertopt
dc.sourceScopus
dc.subjectMetals and alloys
dc.subjectPhase transformations
dc.subjectThermal analysis
dc.titleCharacteristics of the Cu-18.84 at.%Al-10.28 at.%Mn-1.57 at.%Ag alloy after slow cooling from high temperaturesen
dc.typeArtigopt
dspace.entity.typePublication
relation.isOrgUnitOfPublicationbc74a1ce-4c4c-4dad-8378-83962d76c4fd
relation.isOrgUnitOfPublication.latestForDiscoverybc74a1ce-4c4c-4dad-8378-83962d76c4fd
unesp.campusUniversidade Estadual Paulista (UNESP), Instituto de Química, Araraquarapt
unesp.departmentFísico-Química - IQARpt

Arquivos

Pacote original

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
2-s2.0-84939464072.pdf
Tamanho:
1.28 MB
Formato:
Adobe Portable Document Format
Descrição: