Effect of atmosphere on the sintering and grain growth of tin oxide
Carregando...
Fontes externas
Fontes externas
Data
Orientador
Coorientador
Pós-graduação
Curso de graduação
Título da Revista
ISSN da Revista
Título de Volume
Editor
Trans Tech Publications
Tipo
Artigo
Direito de acesso
Acesso restrito
Fontes externas
Fontes externas
Resumo
High purity SnO 2 powder (>99.9%) was compacted in cylindrical pellets and sintered in atmospheres of dry argon, argon with water vapor, oxygen and CO 2 using 10 °C/min up to 1200 °C or isotherms in the range of 1000 to 1200 °C. Time, temperature and sintering atmosphere have large influence on grain growth and low influence on densification of this oxide. Surface diffusion is the dominant mechanism up to 1200 °C and evaporation-condensation is dominant above 1200 °C. The maximum linear shrinkage observed was about 2.0% and attributed to structural rearrangement of particles due to high capillary stresses developed with neighboring particles. © 1999 Trans Tech Publications.
Descrição
Palavras-chave
Idioma
Inglês
Citação
Materials Science Forum, v. 299-300, p. 134-140.