Solvothermal method to obtain europium-doped yttrium oxide

dc.contributor.authorDavolos, Marian Rosaly [UNESP]
dc.contributor.authorFeliciano, S.
dc.contributor.authorPires, Ana Maria [UNESP]
dc.contributor.authorMarques, RFC
dc.contributor.authorJafelicci, M.
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2014-05-20T15:24:38Z
dc.date.available2014-05-20T15:24:38Z
dc.date.issued2003-02-15
dc.description.abstractPure yttrium oxide or mixed with europium oxide (3 at%) were treated in supercritical isopropanolic suspension at 500degreesC for 20 It and filling degree of 50%. Products were supercritically dried and characterized by scanning electron microscopy (SEM), X-ray powder diffraction (XRD), infrared spectroscopy (IR) and luminescence spectroscopy (LS). Particle shape is irregular with an equivalent diameter of ca. 5 mum. Cubic crystalline phase is mainly obtained and hydroxide ion in low concentration is detected by IR vibrational spectrum. Europium in this concentration does not extensively change such observed characteristics from the pure yttrium oxide. Luminescence spectra show that the doped product is a mixture of the two oxides added by oxyhydroxide impurities. Nevertheless, this precursor sample, after being heated at 900degreesC during 1 h, has all characteristics, especially luminescent ones, of the P22 commercial phosphor. (C) 2003 Elsevier B.V. (USA). All rights reserved.en
dc.description.affiliationUNESP, Inst Quim, BR-14801970 Araraquara, SP, Brazil
dc.description.affiliationUnespUNESP, Inst Quim, BR-14801970 Araraquara, SP, Brazil
dc.format.extent268-272
dc.identifierhttp://dx.doi.org/10.1016/S0022-4596(02)00174-3
dc.identifier.citationJournal of Solid State Chemistry. San Diego: Academic Press Inc. Elsevier B.V., v. 171, n. 1-2, p. 268-272, 2003.
dc.identifier.doi10.1016/S0022-4596(02)00174-3
dc.identifier.issn0022-4596
dc.identifier.lattes4284809342546287
dc.identifier.lattes2115942621694174
dc.identifier.urihttp://hdl.handle.net/11449/35214
dc.identifier.wosWOS:000183207400042
dc.language.isoeng
dc.publisherElsevier B.V.
dc.relation.ispartofJournal of Solid State Chemistry
dc.relation.ispartofjcr2.179
dc.relation.ispartofsjr0,632
dc.rights.accessRightsAcesso restrito
dc.sourceWeb of Science
dc.subjectY2O3 : Eupt
dc.subjectsolvothermalpt
dc.subjectisopropanolpt
dc.subjectluminescencept
dc.titleSolvothermal method to obtain europium-doped yttrium oxideen
dc.typeArtigo
dcterms.licensehttp://www.elsevier.com/about/open-access/open-access-policies/article-posting-policy
dcterms.rightsHolderElsevier B.V.
dspace.entity.typePublication
unesp.author.lattes4284809342546287
unesp.author.lattes2115942621694174
unesp.author.lattes5408864375841292[3]
unesp.author.orcid0000-0001-8326-1465[1]
unesp.author.orcid0000-0001-9607-0510[3]
unesp.campusUniversidade Estadual Paulista (UNESP), Instituto de Química, Araraquarapt
unesp.departmentQuímica Inorgânica - IQARpt

Arquivos

Licença do Pacote

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: