Abstract
This paper presents the results of thermogravimetric analysis (TGA) tests in PVC (1.0; 2.0 mm) and HDPE (0.8; 2.5 mm) geomembranes exposed to weathering and leachate after 30 months. The aim of this paper is the comparison of fresh and exposed samples to assess the degradation process concerning the total loss of mass of geomembranes. The exposure was conducted in accordance with the recommendations of ASTM standards. The TGA tests were carried out according to ASTM D6370 and E2105. Results show, for instance, that for PVC geomembrane the largest reductions of plasticizers occurred for samples exposed to weathering. The loss of plasticizers after the exposure contributed to the decrease of deformation and consequent increase in stiffness. TGA tests shows to be a valuable tool to control the quality of the materials. © 2012 ejge.
Description
Keywords
Chemical degradation PVC and HDPE geomembranes TGA tests Weathering ASTM Standards Degradation process Leachates Total loss Vinyl chlorides Chlorine compounds Geomembranes Plasticizers Polyvinyl chlorides Reinforced plastics Solvents Thermogravimetric analysis degradation geomembrane leachate thermogravimetry weathering