CaCu3Ti4O12 (stoichiometric) and Ca1.1Cu2.9Ti4O12 (non-stoichiometric) thin films have been prepared by the soft chemical method on Pt/Ti/SiO2/Si substrates, and their electrical and dielectric properties have been compared as a function of the annealing temperature. The crystalline structure and the surface morphology of the films were markedly affected by the annealing temperature and excess calcium. The films show frequency-independent dielectric properties at room temperature which is similar to those properties obtained in single-crystal or epitaxial thin films. The room temperature dielectric constant of the 570-nm-thick CCTO thin films annealed at 600 degrees C at 10 kHz was found to be 124. The best non-ohmic behavior (alpha = 12.6) presented by the film with excess calcium annealed at 500 degrees C. Resistive hysteresis on the I-V curves was observed which indicates these films can be used in resistance random access memory (ReRAM). Published by Elsevier B.V.

Descrição

Idioma

Inglês

Citação

Journal of Alloys and Compounds. Lausanne: Elsevier B.V. Sa, v. 509, n. 41, p. 9930-9933, 2011.

Itens relacionados

Unidades

Tipo de item:Unidade,
Araraquara, Instituto de Química - IQAR
IQAR
Campus: Araraquara

Tipo de item:Unidade,
Guaratinguetá, Faculdade de Engenharia e Ciências - FEG
FEG
Campus: Guaratinguetá

Departamentos

Cursos de graduação

Programas de pós-graduação