Reduced deactivation of mechanochemically delaminated hierarchical zeolite MCM-22 catalysts during 4-propylphenol cracking
Carregando...
Fontes externas
Fontes externas
Data
Orientador
Coorientador
Pós-graduação
Curso de graduação
Título da Revista
ISSN da Revista
Título de Volume
Editor
Elsevier
Tipo
Artigo
Direito de acesso
Acesso aberto

Fontes externas
Fontes externas
Resumo
The delamination of MCM-22 using shear forces in a vibratory ball mill, rather than chemical surfactants and sonication, is illustrated. The resulting material has comparable or improved physical properties compared to chemically delaminated MCM-22 without a significant loss of acid sites. The mechanical treatment affected the initial rate of 4-propylphenol cracking to phenol and propylene, a model reaction for lignin-derived aromatics, much less than chemical delamination. It also shows improved deactivation resistance for this reaction known to experience fast deactivation by pore blockage.
Descrição
Palavras-chave
Idioma
Inglês
Citação
Journal of Catalysis, v. 411, p. 187-192.