dc.description.abstractO objetivo deste estudo foi comparar, por meio de ensaio de resistência à fadiga, materiais cerâmicos de diferentes graus de dureza para confecção de facetas palatinas no restabelecimento da guia canina em caninos humanos e analisar a tensão superficial por elementos finitos. Foram confeccionados 45 preparos anatômicos padronizados com desgaste uniforme de 1,2 mm de espessura. Os preparos foram escaneados, as restaurações foram desenhadas e fresadas em cerâmica vítrea reforçada por polímero (CVRP, VITA Enamic), cerâmica à base de silicato de lítio reforçado por zircônia (ZLS, VITA Suprinity) ou zircônia tetragonal estabilizada por óxido de ítrio de alta translucidez (YZHT, VITA YZ HT). Os preparos dentais foram condicionados, as restaurações foram tratadas de acordo com as recomendações dos fabricantes, e cimentados adesivamente. Em seguida, 3 espécimes de cada grupo foram testados monotonicamente para determinação dos parâmetros de fadiga. As médias do teste monotônico foram respectivamente para CVRP, ZLS e YZHT os valores de 674,18N, 560,58N e 918,98N. Foi realizado o ensaio de vida acelerado stepwise stress até a fratura dos espécimes ou até a suspensão do ensaio após 1,2 x 106 ciclos. Em relação a sobrevivência, pelo método de Kaplan-Meir, CVRP apresentou resultados para média e mediana de 245,21 e 225, respectivamente; ZLS teve média de 175,76 e mediana de 168 e YZHT com média de 383,30 e mediana de 366. Em relação ao método de Weibull, CVRP apresentou resultados de 5,43 e 264 para forma e escala, respectivamente; ZLS teve 36,14 para forma e 380,67 para escala; e YZHT apresentou 4,95 para forma e 417,38 para escala. As facetas palatinas também foram avaliadas em modelos computacionais por meio da análise de elementos finitos. Sendo calculado maior valor de tensão para YZ HT, ZLS, CVRP respectivamente. É possível concluir que todos os materiais testados apresentam a possibilidade de serem utilizados para reabilitação na face palatina de caninos superiores.pt
dc.description.abstractThe aim of this study was to compare, by means of a fatigue strength test, ceramic materials with different hardness levels to produce palatal veeners to restore canine guide for protection. Forty-five standardized anatomical preparations were made in healthy human canines with uniform 1.2 mm thickness. The samples were scanned, the restorations were designed and milled in polymer infiltrated ceramic network (PICN, VITA Enamic), zirconia-reinforced lithium silicate (ZLS, VITA Suprinity) and high translucent yttrium oxide-reinforced tetragonal zirconia (YZHT, VITA YZ HT). Dental preparations were conditioned, restorations were treated according to the manufacturers' recommendations, and adhesively cemented. Then, 3 samples of each group were monotonically tested to determine the fatigue parameters. The mean of the monotonic test was respectively for PRGC, ZLS and YZHT 674.18N; 560.58N and 918.98N. The stepwise stress accelerated life test (SSALT) was performed until specimen fracture or until suspension of the test after 1.2 x 106 cycles. Regarding survival, using the Kaplan Meir method, PRGC presented results for the mean and median of 245.21 and 225, respectively; ZLS had an average of 175.76 and a median of 168 and YZHT with an average of 383.30 and a median of 366. Regarding the Weibull method, PRGC showed results of 5.43 and 264 for form and scale, respectively; ZLS had 36.14 for form and 380.67 for scale; and YZHT presented 4.95 for form and 417.38 for scale. The palatal veneers were also evaluated in computational models through finite element analysis. The highest voltage value being calculated for YZ HT, ZLS, CVRP respectively. It is possible to conclude that all tested materials have the possibility of being used for rehabilitation on the palatal surface of upper canines.en
dc.identifier.capes33004145070P8
dc.identifier.urihttp://hdl.handle.net/11449/216037
dc.language.isopor
dc.publisherUniversidade Estadual Paulista (Unesp)
dc.rights.accessRightsAcesso aberto
dc.subjectCaninopt
dc.subjectRestauraçãopt
dc.subjectCerâmicaspt
dc.subjectFadigapt
dc.subjectAnálise por elementos finitos.pt
dc.subjectCanine. Restorationpt
dc.subjectCeramicsen
dc.subjectFinite element analysisen
dc.subjectFatigueen
dc.subjectRestorationen
dc.titleEfeito do material restaurador na resistência à fadiga e distribuição de tensão em facetas palatinas em caninos superiorespt
dc.title.alternativeEffect of Different Ceramic Materials on Fatigue Resistance and Stress Distribution in Upper Canines with Palatal Veneersen
dc.typeDissertação de mestrado
unesp.campusUniversidade Estadual Paulista (Unesp), Instituto de Ciência e Tecnologia, São José dos Campospt
unesp.embargoOnlinept
unesp.examinationboard.typeBanca restritapt
unesp.graduateProgramOdontologia Restauradora - ICTpt
unesp.knowledgeAreaPrótese dentáriapt
unesp.researchAreaCerâmicas odontológicaspt

Arquivos

Pacote Original
Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
tanaka_iv_me_sjc.pdf
Tamanho:
5.8 MB
Formato:
Adobe Portable Document Format
Descrição:
Licença do Pacote
Agora exibindo 1 - 1 de 1
Nenhuma Miniatura disponível
Nome:
license.txt
Tamanho:
3.01 KB
Formato:
Item-specific license agreed upon to submission
Descrição: