Publicação: Pre-sintered Y-TZP sandblasting: effect on surface roughness, phase transformation, and Y-TZP/veneer bond strength
dc.contributor.author | Ramos-Tonello, Carla Muller | |
dc.contributor.author | Trevizo, Bruno Freitas | |
dc.contributor.author | Rodrigues, Raphaela Farias | |
dc.contributor.author | Rodrigues Magalhaes, Ana Paula | |
dc.contributor.author | Furuse, Adilson Yoshio | |
dc.contributor.author | Lisboa-Filho, Paulo Noronha [UNESP] | |
dc.contributor.author | Tabata, Americo Sheitiro [UNESP] | |
dc.contributor.author | Sanches Borges, Ana Flavia | |
dc.contributor.institution | Fac Metropolitanas Unidas | |
dc.contributor.institution | Universidade de São Paulo (USP) | |
dc.contributor.institution | Universidade Estadual Paulista (Unesp) | |
dc.date.accessioned | 2018-11-26T17:42:34Z | |
dc.date.available | 2018-11-26T17:42:34Z | |
dc.date.issued | 2017-11-01 | |
dc.description.abstract | Sandblasting is a common method to try to improve the Y-TZP/veneer bond strength of dental prostheses, however, it may put stress on zirconia surfaces and could accelerate the t -> m phase transformation. Y-TZP sandblasting before sintering could be an alternative to improve surface roughness and bonding strength of veneering ceramic. Objectives. The aim of this study was to analyze the effect of Y-TZP pre-sintering sandblasting on surface roughness, phase transformation, and the Y-TZP/veneer shear bond strength. Material and Methods. The Y-TZP specimen surface underwent sandblasting with aluminum oxide (50 mu m) pre-sintering (Z-PRE) and post sintering (Z-POS). Z-CTR was not subjected to surface treatment. After ceramic veneer application, the specimens were subjected to shear bond testing. Surface roughness was analyzed by confocal microscopy. Y-TZP monoclinic and tetragonal phases were evaluated by micro-Raman spectroscopy. Shear bond strength and surface roughness data were analyzed by One-way ANOVA and Tukey tests (alpha=0.05). Differences in the wave numbers and the broadening bands of the Raman spectra were compared among groups. Results. Z-POS (9.73 +/- 5.36 MPa) and Z-PRE (7.94 +/- 2.52 MPa) showed the highest bond strength, significantly higher than that of Z-CTR (5.54 +/- 2.14 MPa). The Ra of Z-PRE (1.59 +/- 0.23 mu m) was much greater and significantly different from that of Z-CTR (0.29 +/- 0.05 mu m) and Z-POS (0.77 +/- 0.13 mu m). All groups showed bands typical of the tetragonal (T) and monoclinic (M) phases. Y-TZP sandblasting before sintering resulted in rougher surfaces but did not increase the shear bond strength compared to post-sintering and increased surface defects. Conclusions. Surface treatment with Al3O2, regardless of the moment and application, improves the results of Y-TZP/veneer bonding and is not a specific cause of t -> m transformation. | en |
dc.description.affiliation | Fac Metropolitanas Unidas, Fac Odontol, Sao Paulo, SP, Brazil | |
dc.description.affiliation | Univ Sao Paulo, Fac Odontol Bauru, Al Octavio Pinheiro Brisola 9-75,Vila Univ, BR-17012901 Bauru, SP, Brazil | |
dc.description.affiliation | Univ Sao Paulo, Fac Odontol Bauru, Dept Dent Endodontia & Mat Dentarios, Bauru, SP, Brazil | |
dc.description.affiliation | Univ Estadual Paulista, Dept Fis, Fac Ciencias, Bauru, SP, Brazil | |
dc.description.affiliationUnesp | Univ Estadual Paulista, Dept Fis, Fac Ciencias, Bauru, SP, Brazil | |
dc.description.sponsorship | Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP) | |
dc.description.sponsorshipId | FAPESP: 2011/18061-0 | |
dc.description.sponsorshipId | FAPESP: 2013/23464-2 | |
dc.format.extent | 666-673 | |
dc.identifier | http://dx.doi.org/10.1590/1678-7757-2017-0131 | |
dc.identifier.citation | Journal Of Applied Oral Science. Bauru-sp: Univ Sao Paulo Fac Odontologia Bauru, v. 25, n. 6, p. 666-673, 2017. | |
dc.identifier.doi | 10.1590/1678-7757-2017-0131 | |
dc.identifier.file | S1678-77572017000600666.pdf | |
dc.identifier.issn | 1678-7757 | |
dc.identifier.lattes | 1353862414532005 | |
dc.identifier.orcid | 0000-0002-7734-4069 | |
dc.identifier.scielo | S1678-77572017000600666 | |
dc.identifier.uri | http://hdl.handle.net/11449/163571 | |
dc.identifier.wos | WOS:000417175900011 | |
dc.language.iso | eng | |
dc.publisher | Univ Sao Paulo Fac Odontologia Bauru | |
dc.relation.ispartof | Journal Of Applied Oral Science | |
dc.relation.ispartofsjr | 0,645 | |
dc.rights.accessRights | Acesso aberto | |
dc.source | Web of Science | |
dc.subject | Zirconium | |
dc.subject | Ceramics | |
dc.subject | Surface properties | |
dc.subject | Shear strength | |
dc.title | Pre-sintered Y-TZP sandblasting: effect on surface roughness, phase transformation, and Y-TZP/veneer bond strength | en |
dc.type | Artigo | |
dcterms.rightsHolder | Univ Sao Paulo Fac Odontologia Bauru | |
dspace.entity.type | Publication | |
unesp.author.lattes | 1353862414532005[6] | |
unesp.author.lattes | 9354064620643611[7] | |
unesp.author.orcid | 0000-0002-7734-4069[6] | |
unesp.author.orcid | 0000-0002-9389-0238[7] | |
unesp.department | Física - FC | pt |
Arquivos
Pacote Original
1 - 1 de 1
Carregando...
- Nome:
- S1678-77572017000600666.pdf
- Tamanho:
- 372.53 KB
- Formato:
- Adobe Portable Document Format