SrBi2Ta2O9 ferroelectric thick films prepared by electrophoretic deposition using aqueous suspension

dc.contributor.authorZanetti, S. M.
dc.contributor.authorVarela, José Arana [UNESP]
dc.contributor.authorLeite, E. R.
dc.contributor.authorLongo, Elson [UNESP]
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.contributor.institutionUniversidade Federal de São Carlos (UFSCar)
dc.date.accessioned2014-05-20T15:24:19Z
dc.date.available2014-05-20T15:24:19Z
dc.date.issued2004-07-01
dc.description.abstractSrBi2Ta2O9 ferroelectric thick films were prepared by electrophoretic deposition (EPD). For that, ceramic powders were prepared by chemical method in order to obtain compounds with chemical homogeneity. The polymeric precursor method was used for the synthesis of the SrBi2Ta2O9 powder. The crystallographic structure of the powder was examined by X-ray diffraction, and the surface area was determined by single point BET adsorption. The 0.03 vol.% suspension was formed by dispersing the powder in water using two different polymers as dispersants: an ester polyphosphate (C213) and an ammonium polyacrilate (Darvan 821-A). It was investigated the influence of the different dispersants in the surface properties of the powder by zeta potential measurements. The films were deposited on platinum-coated alumina and Pt/Ti/SiO2/Si substrates by a 4 mA constant current, for 10 min, using two parallel electrodes placed at a separation distance of 3 min in the suspension. Several cycles of deposition-drying of the deposit were carried out until reaching the desired thickness. After thermal treatment at temperatures ranging from 700 to 1000 degreesC, the films were characterized by X-ray diffraction and scanning electron microscopy for the microstructure observation. (C) 2003 Elsevier Ltd. All rights reserved.en
dc.description.affiliationUNESP, LIEC, Inst Quim, BR-14807455 Araraquara, SP, Brazil
dc.description.affiliationLIEC, Dept Quim, UFSCar, BR-13595905 Sao Carlos, SP, Brazil
dc.description.affiliationUnespUNESP, LIEC, Inst Quim, BR-14807455 Araraquara, SP, Brazil
dc.format.extent2445-2451
dc.identifierhttp://dx.doi.org/10.1016/S0955-2219(03)00633-2
dc.identifier.citationJournal of the European Ceramic Society. Oxford: Elsevier B.V., v. 24, n. 8, p. 2445-2451, 2004.
dc.identifier.doi10.1016/S0955-2219(03)00633-2
dc.identifier.issn0955-2219
dc.identifier.urihttp://hdl.handle.net/11449/34954
dc.identifier.wosWOS:000220335900031
dc.language.isoeng
dc.publisherElsevier B.V.
dc.relation.ispartofJournal of the European Ceramic Society
dc.relation.ispartofjcr3.794
dc.relation.ispartofsjr1,068
dc.rights.accessRightsAcesso restrito
dc.sourceWeb of Science
dc.subjectelectrophoresispt
dc.subjectferroelectric propertiespt
dc.subjectSBTpt
dc.subjectSrBi2Ta2O9pt
dc.subjectsuspensionspt
dc.subjecttantalatespt
dc.subjectthick filmspt
dc.titleSrBi2Ta2O9 ferroelectric thick films prepared by electrophoretic deposition using aqueous suspensionen
dc.typeArtigo
dcterms.licensehttp://www.elsevier.com/about/open-access/open-access-policies/article-posting-policy
dcterms.rightsHolderElsevier B.V.
dspace.entity.typePublication
unesp.campusUniversidade Estadual Paulista (UNESP), Instituto de Química, Araraquarapt
unesp.departmentBioquímica e Tecnologia - IQARpt
unesp.departmentFísico-Química - IQARpt

Arquivos

Licença do Pacote

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: