The influence of a dentin desensitizer on the microtensile bond strength of two bonding systems

dc.contributor.authorSeara, S. F.
dc.contributor.authorErthal, B. S.
dc.contributor.authorRibeiro, M.
dc.contributor.authorKroll, L. [UNESP]
dc.contributor.authorPereira, G. D.S.
dc.contributor.institutionGama Filho School of Dentistry
dc.contributor.institutionUniversidade Estadual de Campinas (UNICAMP)
dc.contributor.institutionGama Filho University
dc.contributor.institutionUniversidade Estadual Paulista (UNESP)
dc.date.accessioned2022-04-28T18:54:37Z
dc.date.available2022-04-28T18:54:37Z
dc.date.issued2002-01-01
dc.description.abstractA laboratory study evaluated the influence of a dentin desensitizer (D/Sense 2) on the microtensile bond strength of two adhesive systems: a self-etching primer (Bistite II SC) and a one-bottle adhesive (Prime & Bond 2.1). Sixteen crown dentin discs were obtained from extracted sound human third molars. Dentin surfaces were ground with 600 grit silicon carbide (SiC) abrasive papers to produce a standardized smear layer. Teeth were randomly divided into four groups (n=4). G1-D/Sense 2 + Prime & Bond 2.1; G2-D/Sense 2 + Bistite II SC; G3- and G4-dentin surfaces were bonded with Prime & Bond 2.1 and Bistite II SC, respectively, with no previous treatment with D/Sense 2. Eight mm high resin composite crowns (TPH Spectrum) were incrementally built-up on the treated surfaces. One sample from each group was prepared for evaluation of the hybrid layer on SEM. The specimens for the microtensile test were serially sectioned perpendicular to the adhesive layer to obtain 1 mm2 bounded sticks. Then, each stick was submitted to the microtensile test performed at a 0.5 mm/min crosshead speed. One-way ANOVA and Tukey test showed statistically significant differences among the groups (p<0.05). Values in MPa were: G1-17.85; G2-9.88; G3-35.16; G4-15.57. Based on the results of this study, it can be concluded that the D/Sense 2 desensitizer decreased the bond strength of Prime & Bond 2.1 and Bistite II SC bonding systems. © Operative Dentistry, 2002.en
dc.description.affiliationDepartment of Restorative Dentistry Gama Filho School of Dentistry
dc.description.affiliationPiracicaba School of Dentistry UNICAMP
dc.description.affiliationGama Filho University, Ribeiro de Almeida 38/1101, Laranjeiras, Rio de Janeiro-RJ
dc.description.affiliationDepartment of Restorative Dentistry Gama Filho School of Dentistry, Carvalho Alvim, 691/1201, Tijuca. Rio de Janeiro-RJ
dc.description.affiliationDepartment of Mathematics Statistic Institute São Paulo State University, Antonia Sabadin Dorniziello, 238, Santa Rita, Piracicaba, SP
dc.description.affiliationUnespDepartment of Mathematics Statistic Institute São Paulo State University, Antonia Sabadin Dorniziello, 238, Santa Rita, Piracicaba, SP
dc.format.extent154-160
dc.identifier.citationOperative Dentistry, v. 27, n. 2, p. 154-160, 2002.
dc.identifier.issn0361-7734
dc.identifier.scopus2-s2.0-0036515196
dc.identifier.urihttp://hdl.handle.net/11449/219266
dc.language.isoeng
dc.relation.ispartofOperative Dentistry
dc.sourceScopus
dc.titleThe influence of a dentin desensitizer on the microtensile bond strength of two bonding systemsen
dc.typeArtigo