Publicação:
Influence of the grinding wheel's dive speed on the damage of rectified hardened steels

dc.contributor.authorAlves, M. C. S. [UNESP]
dc.contributor.authorBianchi, E. C. [UNESP]
dc.contributor.authorAguiar, P. R. [UNESP]
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2014-05-20T13:27:25Z
dc.date.available2014-05-20T13:27:25Z
dc.date.issued2008-01-01
dc.description.abstractThe world tendency is the increase of the productivity and the production of pieces more and more sophisticated, with high degree of geometric and dimensional tolerances, with good surface finish and low cost. Rectification is responsible for the final finish in the machining process of a material. However, damages generated in this production phase affect all the resources used in the previous processes. Great part of the problems happennig in the rectification process is due to the enormous temperature generated in this activity because of the machining conditions. The dive speed, which is directly related to the productivity, is considered responsible for the damages that occur during rectification, limiting its values to those that do not cause such damages. In this work, through the variation of the dive speed in the process of cylindrical grinding of type ABNT D6 steel, rationalizing the application of two cutting fluids and using a CBN (cubic boron nitrate) abrasive wheel with vitrified blond, the influence of the dive speed on the surface damages of hardened steels was evaluated. The results allowed to say that the dive speed, associated to an efficient cooling and lubrication, didn't provoke thermal damages (including heated zones, cracks and tension stresses) to the material. Residual stresses and the roughness of rectified materials presented a correlation with the machining conditions. The work concluded that it is possible to increase the productivity without provoking damages in the rectified components.en
dc.description.affiliationUniv Estadual Paulista, UNESP, Dept Eng Mecan, BR-17033360 Bauru, SP, Brazil
dc.description.affiliationUnespUniv Estadual Paulista, UNESP, Dept Eng Mecan, BR-17033360 Bauru, SP, Brazil
dc.format.extent636-642
dc.identifier.citationMateria-rio de Janeiro. Rio de Janeiro Rj: Univ Fed Rio de Janeiro, Lab Hidrogenio, v. 13, n. 4, p. 636-642, 2008.
dc.identifier.issn1517-7076
dc.identifier.lattes1099152007574921
dc.identifier.lattes1455400309660081
dc.identifier.orcid0000-0002-9934-4465
dc.identifier.urihttp://hdl.handle.net/11449/8997
dc.identifier.wosWOS:000269837000009
dc.language.isopor
dc.publisherUniv Fed Rio de Janeiro, Lab Hidrogenio
dc.relation.ispartofMatéria (Rio de Janeiro)
dc.relation.ispartofjcr0.340
dc.relation.ispartofsjr0,188
dc.rights.accessRightsAcesso aberto
dc.sourceWeb of Science
dc.subjecthardened Steelsen
dc.subjectrectificationen
dc.subjectthermal damagesen
dc.subjectroughnessen
dc.subjectresidual stressesen
dc.subjectgrindingen
dc.subjectdive speeden
dc.titleInfluence of the grinding wheel's dive speed on the damage of rectified hardened steelsen
dc.typeArtigo
dcterms.licensehttp://www.scielo.br/revistas/rmat/paboutj.htm
dcterms.rightsHolderUniv Fed Rio de Janeiro, Lab Hidrogenio
dspace.entity.typePublication
unesp.author.lattes1099152007574921[2]
unesp.author.lattes1455400309660081[3]
unesp.author.orcid0000-0002-9934-4465[3]
unesp.author.orcid0000-0003-2675-4276[2]
unesp.campusUniversidade Estadual Paulista (UNESP), Faculdade de Engenharia, Baurupt
unesp.departmentEngenharia Mecânica - FEBpt

Arquivos

Licença do Pacote

Agora exibindo 1 - 2 de 2
Nenhuma Miniatura disponível
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição:
Nenhuma Miniatura disponível
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: