Improvement of the chemical resistance of zirconium fluoride glasses coated with a Tiron (R) modified tin oxide layer prepared by the sol-gel process

dc.contributor.authorHammer, Peter [UNESP]
dc.contributor.authorRizzato, A. P.
dc.contributor.authorSantilli, Celso Valentim [UNESP]
dc.contributor.authorPulcinelli, Sandra Helena [UNESP]
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2014-05-20T15:27:27Z
dc.date.available2014-05-20T15:27:27Z
dc.date.issued2006-09-15
dc.description.abstractIn order to improve the chemical resistance of zirconium fluoride glass a protective transparent SnO2 layer was deposited by the solgel dip-coating process in the presence of Tiron (R) as particle surface modifier agent. After water immersion for different periods of time, both coated and non-coated fluoride glasses were analyzed by scanning electron microscopy, mass loss evaluation, infrared spectroscopy and X-ray photoelectron spectroscopy. In contrast to the effects occurring for non-coated glass, where the surface undergoes a rapid selective dissolution of the most soluble species, the results for the SnO2-coated glass showed that the filling of the film nanopores by dissolved glass material results in a hermetic barrier protecting the glass surface. The selective glass dissolution was confirmed by liquid chromatography measurements of the etching solution after each exposure time. (c) 2006 Elsevier B.V. All rights reserved.en
dc.description.affiliationUNESP, Inst Quim, BR-14801970 Araraquara, SP, Brazil
dc.description.affiliationUnespUNESP, Inst Quim, BR-14801970 Araraquara, SP, Brazil
dc.format.extent3653-3658
dc.identifierhttp://dx.doi.org/10.1016/j.jnoncrysol.2006.03.098
dc.identifier.citationJournal of Non-crystalline Solids. Amsterdam: Elsevier B.V., v. 352, n. 32-35, p. 3653-3658, 2006.
dc.identifier.doi10.1016/j.jnoncrysol.2006.03.098
dc.identifier.issn0022-3093
dc.identifier.lattes6466841023506131
dc.identifier.lattes5584298681870865
dc.identifier.lattes9971202585286967
dc.identifier.orcid0000-0002-3823-0050
dc.identifier.orcid0000-0002-8356-8093
dc.identifier.urihttp://hdl.handle.net/11449/37430
dc.identifier.wosWOS:000240706000050
dc.language.isoeng
dc.publisherElsevier B.V.
dc.relation.ispartofJournal of Non-Crystalline Solids
dc.relation.ispartofjcr2.488
dc.relation.ispartofsjr0,722
dc.rights.accessRightsAcesso restrito
dc.sourceWeb of Science
dc.subjectchemical durabilitypt
dc.subjectcorrosionpt
dc.subjectflims and coatingspt
dc.subjectinfrared glassespt
dc.subjectfluoridespt
dc.subjectscanning electron microscopypt
dc.subjectnanoparticlespt
dc.subjectFTIR measurementspt
dc.subjecttin oxidept
dc.subjectXPSpt
dc.titleImprovement of the chemical resistance of zirconium fluoride glasses coated with a Tiron (R) modified tin oxide layer prepared by the sol-gel processen
dc.typeArtigo
dcterms.licensehttp://www.elsevier.com/about/open-access/open-access-policies/article-posting-policy
dcterms.rightsHolderElsevier B.V.
dspace.entity.typePublication
unesp.author.lattes6466841023506131(1)
unesp.author.lattes9971202585286967
unesp.author.lattes5584298681870865[3]
unesp.author.orcid0000-0002-3823-0050(1)
unesp.author.orcid0000-0002-8356-8093[3]
unesp.campusUniversidade Estadual Paulista (UNESP), Instituto de Química, Araraquarapt
unesp.departmentFísico-Química - IQARpt

Arquivos

Licença do Pacote

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: