Publicação: BOND STRENGTH DURABILITY of SELF-ETCHING ADHESIVES and RESIN CEMENTS TO DENTIN
dc.contributor.author | Lima Chaves, Carolina de Andrade [UNESP] | |
dc.contributor.author | de Melo, Renata Marques | |
dc.contributor.author | Passos, Sheila Pestana | |
dc.contributor.author | Camargo, Fernanda Pelogia [UNESP] | |
dc.contributor.author | Bottino, Marco Antonio | |
dc.contributor.author | Balducci, Ivan [UNESP] | |
dc.contributor.institution | Universidade Estadual Paulista (Unesp) | |
dc.date.accessioned | 2014-05-20T14:05:28Z | |
dc.date.available | 2014-05-20T14:05:28Z | |
dc.date.issued | 2009-05-01 | |
dc.description.abstract | Objectives: To evaluate the microtensile bond strength (mu TBS) of one-(Xeno III, Dentsply) and two-step (Tyrian-One Step Plus, Bisco) self-etching adhesive systems bonded to dentin and cemented to chemically cured (C&B Metabond) or light-cured paste of a dual-cure resin cement (Variolink II, Ivoclar) within a short (24 h) and long period of evaluation (90 days). Material and Methods: Forty recently extracted human molars had their roots removed and their occlusal dentin exposed and ground wet with 600-grit SiC paper. After application of one of the adhesives, the resin cement was applied to the bonded surface and a composite resin block was incrementally built up to a height of 5 mm (n = 10). The restored teeth were stored in distilled water at 37 C for 7 days. The teeth were then cut along two axes (x and y), producing beam-shaped specimens with 0.8 mm(2) cross-sectional area, which were subjected to mu TBS testing at a crosshead speed of 0.05 mm/min and stressed to failure after 24 h or 90 days of storage in water. The mu TBS data in MPa were subjected to three-way analysis of variance and Tukey's test (alpha = 0.05). Results: The interaction effect for all three factors was statistically significant (three-way ANOVA, p < 0.001). All eight experimental means (MPa) were compared by the Tukey's test (p < 0.05) and the following results were obtained: Tyrian-One Step Plus /C&B/24 h (22.4 +/- 7.3); Tyrian-One Step Plus /Variolink II/24 h (39.4 +/- 11.6); Xeno III/C&B/24 h (40.3 +/- 12.9); Xeno III/Variolink II/24 h (25.8 +/- 10.5); Tyrian-One Step Plus / C&B/90 d (22.1 +/- 12.8) Tyrian-One Step Plus/VariolinkII/90 d (24.2 +/- 14.2); Xeno III/C&B/90 d (27.0 +/- 13.5); Xeno III/Variolink II/90 d (33.0 +/- 8.9). Conclusions: Xeno III/Variolink II was the luting agent/adhesive combination that provided the most promising bond strength after 90 days of storage in water. | en |
dc.description.affiliation | São Paulo State Univ, Dent Sch Sao Jose dos Campos, Dept Community Sci & Pediat Dent, Sao Jose Dos Campos, SP, Brazil | |
dc.description.affiliation | São Paulo State Univ, Dent Sch Araraquara, Araraquara, SP, Brazil | |
dc.description.affiliation | Dent Sch Sao Jose dos Campos, Dept Dent Mat & Prosthodont, Sao Jose Dos Campos, SP, Brazil | |
dc.description.affiliationUnesp | São Paulo State Univ, Dent Sch Sao Jose dos Campos, Dept Community Sci & Pediat Dent, Sao Jose Dos Campos, SP, Brazil | |
dc.description.affiliationUnesp | São Paulo State Univ, Dent Sch Araraquara, Araraquara, SP, Brazil | |
dc.format.extent | 155-160 | |
dc.identifier | http://dx.doi.org/10.1590/S1678-77572009000300005 | |
dc.identifier.citation | Journal of Applied Oral Science. Bauru-sp: Univ São Paulo Fac Odontologia Bauru, v. 17, n. 3, p. 155-160, 2009. | |
dc.identifier.file | S1678-77572009000300005.pdf | |
dc.identifier.issn | 1678-7757 | |
dc.identifier.lattes | 9234456003563666 | |
dc.identifier.scielo | S1678-77572009000300005 | |
dc.identifier.uri | http://hdl.handle.net/11449/22975 | |
dc.identifier.wos | WOS:000266689200005 | |
dc.language.iso | eng | |
dc.publisher | Universidade de São Paulo (USP), Faculdade de Odontologia de Bauru | |
dc.relation.ispartof | Journal of Applied Oral Science | |
dc.relation.ispartofjcr | 1.709 | |
dc.relation.ispartofsjr | 0,645 | |
dc.rights.accessRights | Acesso aberto | |
dc.source | Web of Science | |
dc.subject | Self-etching adhesives | en |
dc.subject | Resin cements | en |
dc.subject | Durability | en |
dc.subject | Bond strength | en |
dc.subject | Microtensile testing | en |
dc.title | BOND STRENGTH DURABILITY of SELF-ETCHING ADHESIVES and RESIN CEMENTS TO DENTIN | en |
dc.type | Artigo | |
dcterms.license | http://www.scielo.br/revistas/jaos/paboutj.htm | |
dcterms.rightsHolder | Univ São Paulo Fac Odontologia Bauru | |
dspace.entity.type | Publication | |
unesp.author.lattes | 9234456003563666 | |
unesp.campus | Universidade Estadual Paulista (UNESP), Instituto de Ciência e Tecnologia, São José dos Campos | pt |
unesp.department | Odontologia Social e Clínica Infantil - ICT | pt |
Arquivos
Pacote Original
1 - 1 de 1
Carregando...
- Nome:
- S1678-77572009000300005.pdf
- Tamanho:
- 700.56 KB
- Formato:
- Adobe Portable Document Format
- Descrição:
Licença do Pacote
1 - 2 de 2
Carregando...
- Nome:
- license.txt
- Tamanho:
- 1.71 KB
- Formato:
- Item-specific license agreed upon to submission
- Descrição:
Carregando...
- Nome:
- license.txt
- Tamanho:
- 1.71 KB
- Formato:
- Item-specific license agreed upon to submission
- Descrição: