Effect of metal conditioners on the adhesive bonding of resin cements to cast titanium

dc.contributor.authorda Rocha, Sickran Soares
dc.contributor.authorAdabo, Gelson Luis [UNESP]
dc.contributor.authorSpinola, Sandra Gouveia
dc.contributor.authorFonseca, Renata Garcia [UNESP]
dc.contributor.authorFerreira, Arlelise Rodolfo
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.contributor.institutionPaulista Univ UNIP
dc.date.accessioned2014-05-20T13:46:18Z
dc.date.available2014-05-20T13:46:18Z
dc.date.issued2007-09-01
dc.description.abstractObjective: To assess the effect of metal conditioners on the bond strength between resin cements and cast titanium. Method and Materials: Commercially pure titanium (99.56%) was cast using an arc casting machine. Surfaces were finished with 400-grit silicon carbide paper followed by air abrasion with 50-mu m aluminum oxide. A piece of double-coated tape with a 4-mm circular hole was then positioned on the metal surface to control the area of the bond. The prepared surfaces were then divided into 4 groups (n=10): G1, unprimed Panavia F; G2, Alloy Primer-Panavia F; G3, unprimed Bistite DC; G4, Metaltite-Bistite DC. Forty minutes after insertion of the resin cements, the specimens were detached from the mold and stored in water at 37 C for 24 hours. Shear bond strength was performed in a testing machine (MTS 810) at a crosshead speed of 0.5 mm/min. Data were analyzed using ANOVA and Tukey's test with a .05 significance level. The fractured surfaces were observed through an optical microscope at 10x magnification. Results: the G1 group demonstrated significantly higher shear bond strength (17.95 MPa) than the other groups. G3 (13.79 MPa) and G4 (12.98 MPa) showed similar mean values to each other and were statistically superior to G2 (9.31 MPa). Debonded surfaces generally presented adhesive failure between metal surfaces and resin cements. Conclusion: While the Metaltite conditioner did not influence the bond strength of the Bistite DC cement, the Alloy Primer conditioner significantly decreased the mean bond strength of the Panavia F cement.en
dc.description.affiliationSao Paolo State Univ UNESP, Dept Dent Mat & Prosthodont, BR-14801903 Araraquara, SP, Brazil
dc.description.affiliationPaulista Univ UNIP, Hlth Sci Inst, Goiania, Go, Brazil
dc.description.affiliationUnespSao Paolo State Univ UNESP, Dept Dent Mat & Prosthodont, BR-14801903 Araraquara, SP, Brazil
dc.format.extentE506-E510
dc.identifierhttp://www.quintpub.com/journals/qi/abstract.php?article_id=2951#.UulZ6LRTvIU
dc.identifier.citationQuintessence International. Hanover Park: Quintessence Publishing Co Inc., v. 38, n. 8, p. E506-E510, 2007.
dc.identifier.issn0033-6572
dc.identifier.lattes2851339311179809
dc.identifier.lattes3041561340615890
dc.identifier.urihttp://hdl.handle.net/11449/16374
dc.identifier.wosWOS:000248726700010
dc.language.isoeng
dc.publisherQuintessence Publishing Co Inc
dc.relation.ispartofQuintessence International
dc.relation.ispartofjcr1.088
dc.relation.ispartofsjr0,563
dc.rights.accessRightsAcesso restritopt
dc.sourceWeb of Science
dc.subjectfixed partial denturept
dc.subjectmetal conditionerspt
dc.subjectresin cementspt
dc.subjectshear bond strengthpt
dc.subjecttitaniumpt
dc.titleEffect of metal conditioners on the adhesive bonding of resin cements to cast titaniumen
dc.typeArtigopt
dcterms.licensehttp://www.quintpub.com/terms.php
dcterms.rightsHolderQuintessence Publishing Co Inc
dspace.entity.typePublication
relation.isDepartmentOfPublication3936e2e2-946a-42ab-8b9d-9521513200fc
relation.isDepartmentOfPublication.latestForDiscovery3936e2e2-946a-42ab-8b9d-9521513200fc
relation.isOrgUnitOfPublicationca4c0298-cd82-48ee-a9c8-c97704bac2b0
relation.isOrgUnitOfPublication.latestForDiscoveryca4c0298-cd82-48ee-a9c8-c97704bac2b0
unesp.author.lattes2851339311179809
unesp.author.lattes3041561340615890
unesp.author.orcid0000-0002-0734-7926[2]
unesp.author.orcid0000-0001-6657-913X[4]
unesp.campusUniversidade Estadual Paulista (UNESP), Faculdade de Odontologia, Araraquarapt
unesp.departmentMateriais Odontológicos e Prótese - FOARpt

Arquivos

Licença do Pacote

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: