Does Adhesive Resin Application Contribute to Resin Bond Durability on Etched and Silanized Feldspathic Ceramic?
dc.contributor.author | Passos, Sheila Pestana [UNESP] | |
dc.contributor.author | Valandro, Luiz Felipe | |
dc.contributor.author | Amaral, Regina [UNESP] | |
dc.contributor.author | Ozcan, Mutlu | |
dc.contributor.author | Bottino, Marco Antonio [UNESP] | |
dc.contributor.author | Kimpara, Estevão Tomomitsu [UNESP] | |
dc.contributor.institution | Universidade Federal de Santa Maria (UFSM) | |
dc.contributor.institution | Universidade Estadual Paulista (Unesp) | |
dc.contributor.institution | University of Groningen | |
dc.date.accessioned | 2014-05-20T14:05:00Z | |
dc.date.available | 2014-05-20T14:05:00Z | |
dc.date.issued | 2008-12-01 | |
dc.description.abstract | Purpose: To assess the effect of adhesive application and aging on the bond durability of resin cement to etched and silanized feldspathic ceramic.Materials and Methods: Twenty blocks (6.4 x 6.4 x 4.8 mm) of feldspathic ceramic (Vita VM7) were produced. The ceramic surfaces were conditioned with 10% hydrofluoric acid gel for 60 s and silanized. They were then randomly divided into two groups. While half of the group received no adhesive, in the other half, a layer of adhesive (Scotchbond Multi-Purpose Plus) was applied. Each ceramic block was then placed in its silicone mold with the treated surface exposed. The dual-cured resin cement (Variolink 11) was injected into the mold over the treated surface and polymerized. Specimens were sectioned to achieve nontrimmed bar specimens (approximately 12 sticks/block) that were randomly divided into 2 groups: a) non-aged - microtensile bond test immediately after sectioning; b) aged-thermocycling (TC) 12,000 times, 5 degrees C to 55 degrees C, and water storage (50 days). The microtensile bond strength test was performed in a universal testing machine (crosshead speed: 1 mm/min). The failure types were examined using an optical light microscope and SEM. Bond strength results were analyzed using two-way ANOVA and Tukey's test (alpha = 0.05).Results: The adhesive application affected the bond strength results significantly (p = 0.0001) (without adhesive > with adhesive). While aging conditions did not reduce the bond strength in the groups that received no adhesive (20 +/- 5.3 MPa non-aged and 21.5 +/- 5.6 aged) (p = 0.1698), it significantly affected the bond strength results of the group with adhesive application (18 +/- 4.4 MPa to 14.4 +/- 4.7 MPa) (p < 0.001). All groups showed mainly mixed type of failures between the ceramic and the resin cement (81% to 100%). The group in which no adhesive was applied presented a higher incidence of cohesive failure of ceramic after aging (18%) than those of the other groups.Conclusion: The use of adhesive did not improve resin cement adhesion to the etched and silanized feldspathic ceramic after long-term thermocycling and water storage. | en |
dc.description.affiliation | Universidade Federal de Santa Maria (UFSM), Sch Dent, Dept Restorat Dent, Div Prosthodont, BR-97015372 Santa Maria, RS, Brazil | |
dc.description.affiliation | São Paulo State Univ Sao Jose Campos, Dept Dent Mat & Prosthodont, São Paulo, Brazil | |
dc.description.affiliation | Univ Groningen, Univ Med Ctr Groningen, Dept Dent & Dent Hyg, Groningen, Netherlands | |
dc.description.affiliationUnesp | São Paulo State Univ Sao Jose Campos, Dept Dent Mat & Prosthodont, São Paulo, Brazil | |
dc.description.sponsorship | Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES) | |
dc.format.extent | 455-460 | |
dc.identifier | http://dx.doi.org/10.3290/j.jad.a14148 | |
dc.identifier.citation | Journal of Adhesive Dentistry. Hanover Park: Quintessence Publishing Co Inc, v. 10, n. 6, p. 455-460, 2008. | |
dc.identifier.doi | 10.3290/j.jad.a14148 | |
dc.identifier.issn | 1461-5185 | |
dc.identifier.lattes | 9234456003563666 | |
dc.identifier.lattes | 0967916388665754 | |
dc.identifier.orcid | 0000-0003-0586-4644 | |
dc.identifier.uri | http://hdl.handle.net/11449/22796 | |
dc.identifier.wos | WOS:000263248500007 | |
dc.language.iso | eng | |
dc.publisher | Quintessence Publishing Co Inc | |
dc.relation.ispartof | Journal of Adhesive Dentistry | |
dc.relation.ispartofjcr | 1.691 | |
dc.relation.ispartofsjr | 0,839 | |
dc.rights.accessRights | Acesso restrito | |
dc.source | Web of Science | |
dc.subject | acid etching | en |
dc.subject | bond durability | en |
dc.subject | glass ceramic | en |
dc.subject | microtensile test | en |
dc.subject | resin cement | en |
dc.title | Does Adhesive Resin Application Contribute to Resin Bond Durability on Etched and Silanized Feldspathic Ceramic? | en |
dc.type | Artigo | |
dcterms.license | http://www.quintpub.com/journals/jad/permissions.php | |
dcterms.rightsHolder | Quintessence Publishing Co Inc | |
unesp.author.lattes | 9234456003563666 | |
unesp.author.lattes | 0967916388665754[6] | |
unesp.author.orcid | 0000-0003-0586-4644[6] | |
unesp.campus | Universidade Estadual Paulista (Unesp), Instituto de Ciência e Tecnologia, São José dos Campos | pt |
unesp.department | Materiais Odontológicos e Prótese - ICT | pt |
Arquivos
Licença do Pacote
1 - 2 de 2
Nenhuma Miniatura disponível
- Nome:
- license.txt
- Tamanho:
- 1.71 KB
- Formato:
- Item-specific license agreed upon to submission
- Descrição:
Nenhuma Miniatura disponível
- Nome:
- license.txt
- Tamanho:
- 1.71 KB
- Formato:
- Item-specific license agreed upon to submission
- Descrição: