Tear Strength Analysis of MDX4-4210 and A-2186 Silicones with Different Intrinsic Pigments Incorporated by Mechanical and Industrial Methods

dc.contributor.authorGoiato, Marcelo Coelho [UNESP]
dc.contributor.authorNobrega, Adhara Smith [UNESP]
dc.contributor.authorFreitas Da Silva, Emily Vivianne [UNESP]
dc.contributor.authorMicheline Dos Santos, Daniela [UNESP]
dc.contributor.authorPinheiro De Magalhães Bertoz, André [UNESP]
dc.contributor.authorSonego, Mariana Vilela [UNESP]
dc.contributor.authorDe Moraes Melo Neto, Clovis Lamartine [UNESP]
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2020-12-12T01:52:22Z
dc.date.available2020-12-12T01:52:22Z
dc.date.issued2019-01-01
dc.description.abstractObjective. The aim of this study was to evaluate the tear strength of MDX4-4210 and A-2186 silicones with different intrinsic pigments incorporated by mechanical and industrial methods, comparing nonaged and aged groups. Materials and Methods. Twenty-four groups were created according to the American Society for Testing and Materials D-624/type C, half nonaged and half aged (n = 10): bronze mechanical MDX4-4210, bronze industrial MDX4-4210, black mechanical MDX4-4210, black industrial MDX4-4210, pink mechanical MDX4-4210, pink industrial MDX4-4210, bronze mechanical A-2186, bronze industrial A-2186, black mechanical A-2186, black industrial A-2186, pink mechanical A-2186, and pink industrial A-2186. All specimens were submitted to tear strength analysis. Data were submitted to the ANOVA and Tukey test (p<0.05). Results. An increase in the tear strength values was observed only for the bronze and black MDX4-4210, comparing nonaged and aged silicones (p<0.05), regardless of the manufacturing method. There was a difference in all comparisons between MDX4-4210 and A-2186 silicones with the same pigment type (p<0.05), regardless of the manufacturing method. In all cases, there was no difference in the manufacturing method comparing the MDX4-4210 or A-2186 groups with the same pigment. Conclusion. Accelerated aging did not influence the tear strength in all aged A-2186 silicones and in aged pink industrial and mechanical MDX4-4210 silicones. The other MDX4-4210 groups had an increase in the results after aging. In all cases compared, the A-2186 groups had higher tear strength values than the MDX4-4210 groups. Mechanical and industrial methods can be used for silicone preparation, without changing the tear strength.en
dc.description.affiliationAracatuba Dental School São Paulo State University (UNESP) Bucal Oncology Center
dc.description.affiliationAracatuba Dental School São Paulo State University (UNESP) Department of Dental Materials and Prosthodontics
dc.description.affiliationAracatuba Dental School São Paulo State University (UNESP) Department of Pediatric and Social Dentistry
dc.description.affiliationUnespAracatuba Dental School São Paulo State University (UNESP) Bucal Oncology Center
dc.description.affiliationUnespAracatuba Dental School São Paulo State University (UNESP) Department of Dental Materials and Prosthodontics
dc.description.affiliationUnespAracatuba Dental School São Paulo State University (UNESP) Department of Pediatric and Social Dentistry
dc.identifierhttp://dx.doi.org/10.1155/2019/2573095
dc.identifier.citationInternational Journal of Dentistry, v. 2019.
dc.identifier.doi10.1155/2019/2573095
dc.identifier.issn1687-8736
dc.identifier.issn1687-8728
dc.identifier.scopus2-s2.0-85077460047
dc.identifier.urihttp://hdl.handle.net/11449/199903
dc.language.isoeng
dc.relation.ispartofInternational Journal of Dentistry
dc.sourceScopus
dc.titleTear Strength Analysis of MDX4-4210 and A-2186 Silicones with Different Intrinsic Pigments Incorporated by Mechanical and Industrial Methodsen