Purpose: The adhesiveness of six root canal sealers: Acroseal, Endo CPM, Epiphany, White MTA, Sealapex and Sealer 26 to dentin, was evaluated in a push-out test design. Methods: Twenty eight roots of freshly extracted teeth were gauged with a size 5 Largo drill. With a cutting machine slices of 2 mm were prepared, rinsed with 5.25% NaOCl and a final rinse with 17% EDTA, dried and filled with one of the sealers. After setting their bond strength was measured in a mechanical testing machine. The data were statistically analyzed by using a One Way ANOVA and post hoc Tukey test. Results: The mean and standard deviation from values of bond strength was: Sealapex 2.2±0.4; Endo CPM 3.8±1.3; White MTA 6.0±1.4; Epiphany 10.9±2.6; Sealer 26 12.3±2.3; and Acroseal 12.2±1.4. Acroseal, Sealer 26 and Epiphany presented a significantly (P<0.01) greater bond strength compared with the other sealers. Also White MTA showed higher adhesiveness compared with Endo CPM and Sealapex (P<0.01). Conclusion: The bond strength between endodontic sealers and root dentin was maximal when Acroseal, Sealer 26 and Epiphany were used; Sealapex e Endo CPM, in turn, presented the lowest bond strength mean values. Copyright: © 2012 Bier et al.; licensee EDIPUCRS.
Descrição
Palavras-chave
Dental bonding, Endodontics, Root canal filling materials
Idioma
Inglês
Como citar
Revista Odonto Ciencia, v. 27, n. 4, p. 320-324, 2012.