Comparative in vitro study of the shear bond strength of brackets bonded with restorative and orthodontic resins
Loading...
External sources
External sources
Date
Advisor
Coadvisor
Graduate program
Undergraduate course
Journal Title
Journal ISSN
Volume Title
Publisher
Type
Article
Access right
External sources
External sources
Abstract
The aim of this study was to evaluate the shear bond strength of brackets bonded with different restorative systems and compare it with that afforded by an established orthodontic bonding system. Seventy human bicuspids were used, divided into five different groups with 14 teeth each. Whereas a specific orthodontic bonding resin (TransbondTM XT) was used in the control group, the restorative systems Charisma, Tetric Ceram, TPH Spectrum and Z100 were used in the other four groups. Seven days after bonding the brackets to the samples, shear forces were applied under pressure in a universal testing machine. The data collected was evaluated using the ANOVA test and, when a difference was identified, the Tukey test was applied. A 5% level of significance was adopted. The mean results of the shear bond strength tests were as follows: Group 1 (Charisma), 14.98 MPa; Group 2 (Tetric Ceram), 15.16 MPa; Group 3 (TPH), 17.70 MPa; Group 4 (Z100), 13.91 MPa; and Group 5 or control group (TransbondTM XT), 17.15 MPa. No statistically significant difference was found among the groups. It was concluded that all tested resins have sufficient bond strength to be recommended for bonding orthodontic brackets.
Description
Keywords
Language
English
Citation
Brazilian Oral Research, v. 25, n. 1, p. 49-55, 2011.