Logotipo do repositório
 

Publicação:
Cross-linked dry bonding: A new etch-and-rinse technique

dc.contributor.authorZhou, Jianfeng
dc.contributor.authorChiba, Ayaka
dc.contributor.authorScheffel, Debora L.S. [UNESP]
dc.contributor.authorHebling, Josimeri [UNESP]
dc.contributor.authorAgee, Kelli
dc.contributor.authorTagami, Junji
dc.contributor.authorTan, Jianquo
dc.contributor.authorAbuelenain, Dalia
dc.contributor.authorNawareg, Manar Abu
dc.contributor.authorHassan, Ali H.
dc.contributor.authorBreschi, Lorenzo
dc.contributor.authorTay, Franklin R.
dc.contributor.authorPashley, David H.
dc.contributor.institutionPeking University School and Hospital of Stomatology
dc.contributor.institutionTokyo Medical and Dental University
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.contributor.institutionAugusta University
dc.contributor.institutionKing Abdulaziz University
dc.contributor.institutionUniversity of Bologna and IGM-CNR Unit of Bologna
dc.date.accessioned2018-12-11T17:06:33Z
dc.date.available2018-12-11T17:06:33Z
dc.date.issued2016-09-01
dc.description.abstractObjective To determine if acid-etched, cross-linked dentin can be dehydrated without lowering bond strength below that of cross-linked wet-bonded dentin in vitro. Methods Using extracted human third molars, control acid-etched dentin was bonded with Single Bond Plus, using either the wet- or dry-bonding technique. Experimental acid-etched dentin was treated with 5 mass% grape seed extract (GSE) in different solvents for 1 min before undergoing wet vs dry resin-dentin bonding with Single Bond Plus. Completely demineralized dentin beams were treated with 5% GSE for 0, 1 or 10 min, before measuring stiffness by 3-point flexure. Other completely demineralized beams were treated similarly and then incubated in buffer for 1 week to measure the collagen solubilization by endogenous dentin proteases. Results 24 h microtensile bond strengths (μTBS) in wet and dry controls were 53.5 ± 3.6 and 9.4 ± 1.8 MPa, respectively (p < 0.05). 5% GSE in water gave μTBS of 53.7 ± 3.4 and 39.1 ± 9.7 MPa (p < 0.05), respectively, while 5% GSE in ethanol gave μTBS of 51.2 ± 2.3 and 35.3 ± 2.0 MPa (p < 0.05). 5% GSE in 5% EtOH/95% water gave wet and dry μTBS of 53.0 ± 2.3 and 55.7 ± 5.1 MPa (p > 0.05). Cross-linking demineralized dentin with 5% GSE increased stiffness of dentin and decreased collagen degradation (p < 0.05). Significance 5% GSE pretreatment of acid-etched dentin for 1 min permits the dentin to be completely air-dried without lowering bond strength.en
dc.description.affiliationDepartment of Prosthodontics Peking University School and Hospital of Stomatology
dc.description.affiliationDepartment of Cariology and Operative Dentistry Graduate School of Medical and Dental Sciences Tokyo Medical and Dental University
dc.description.affiliationDepartment of Orthodontics and Pediatric Dentistry Universidade Estadual Paulista-UNESP Araraquara Dental School
dc.description.affiliationDepartment of Oral Biology The Dental College of Georgia Augusta University
dc.description.affiliationFaculty of Dentistry King Abdulaziz University
dc.description.affiliationDepartment of Biomedical and Neuromotor Sciences DIBINEM University of Bologna and IGM-CNR Unit of Bologna
dc.description.affiliationDepartment of Endodontics The Dental College of Georgia Augusta University
dc.description.affiliationUnespDepartment of Orthodontics and Pediatric Dentistry Universidade Estadual Paulista-UNESP Araraquara Dental School
dc.description.sponsorshipFundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
dc.description.sponsorshipNational Institute of Dental and Craniofacial Research
dc.description.sponsorshipIdFAPESP: 2014/17232-4
dc.description.sponsorshipIdFAPESP: 2014/18160-7
dc.description.sponsorshipIdNational Institute of Dental and Craniofacial Research: R01 DE015306
dc.format.extent1124-1132
dc.identifierhttp://dx.doi.org/10.1016/j.dental.2016.06.014
dc.identifier.citationDental Materials, v. 32, n. 9, p. 1124-1132, 2016.
dc.identifier.doi10.1016/j.dental.2016.06.014
dc.identifier.file2-s2.0-84990852406.pdf
dc.identifier.issn0109-5641
dc.identifier.scopus2-s2.0-84990852406
dc.identifier.urihttp://hdl.handle.net/11449/173577
dc.language.isoeng
dc.relation.ispartofDental Materials
dc.relation.ispartofsjr2,106
dc.rights.accessRightsAcesso abertopt
dc.sourceScopus
dc.subjectBond strength
dc.subjectCollagen degradation
dc.subjectCross-linking
dc.subjectDentin
dc.subjectDentin bonding
dc.subjectDentin stiffness
dc.subjectDry bonding
dc.subjectGrape seed extract
dc.subjectWet bonding
dc.titleCross-linked dry bonding: A new etch-and-rinse techniqueen
dc.typeArtigopt
dspace.entity.typePublication
relation.isOrgUnitOfPublicationca4c0298-cd82-48ee-a9c8-c97704bac2b0
relation.isOrgUnitOfPublication.latestForDiscoveryca4c0298-cd82-48ee-a9c8-c97704bac2b0
unesp.campusUniversidade Estadual Paulista (UNESP), Faculdade de Odontologia, Araraquarapt
unesp.departmentClínica Infantil - FOARpt

Arquivos

Pacote Original

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
2-s2.0-84990852406.pdf
Tamanho:
1.63 MB
Formato:
Adobe Portable Document Format
Descrição: