Can Application of Universal Primers Alone Be a Substitute for Airborne-Particle Abrasion to Improve Adhesion of Resin Cement to Zirconia?

dc.contributor.authorPereira, Laudenice de Lucena
dc.contributor.authorCampos, Fernanda [UNESP]
dc.contributor.authorOliveira Dal Piva, Amanda Maria de
dc.contributor.authorGondim, Laisa Daniel
dc.contributor.authorAssuncao e Souza, Rodrigo Othavio de
dc.contributor.authorOezcan, Mutlu
dc.contributor.institutionFed Univ Rio Grande Norte UFRN
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.contributor.institutionUniversidade Federal da Paraíba (UFPB)
dc.contributor.institutionUniv Fed Rio Grande do Norte
dc.contributor.institutionUniv Zurich
dc.date.accessioned2015-10-21T13:15:16Z
dc.date.available2015-10-21T13:15:16Z
dc.date.issued2015-01-01
dc.description.abstractPurpose: To determine whether universal primers alone can deliver similar levels of adhesion of resin cement to zirconia ceramic when compared to their application in conjunction with airborne-particle abrasion.Materials and Methods: Sintered zirconia blocks (N = 160) (Lava, 3M ESPE), (5.25 x 5.25 x 3 mm(3)) were embedded in acrylic resin, polished, and randomly distributed into 16 groups (n = 10 per group), according to the factors "universal primer" (8 levels) and "air-particle abrasion" (2 levels): 1. ctr: control, without application of a universal primer; 2. AP: Alloy Primer; 3. MP: Monobond Plus; 4. MZP: Metal Zirconia Primer; 5. MZ: MZ Primer; 6. Sg: Signum Zirconia Bond; 7. SbU: Singlebond Universal; 8. ZP: Z Prime Plus. The universal primers were also used after air abrasion (A) of zirconia to form the following 8 groups: Ctr-A, AP-A, MP-A, MZP-A, MZ-A, Sg-A, SbU-A, and ZP-A. After ultrasonic cleaning, air abrasion was performed using Al2O3 particles (110 mu m, 2.5 bar, 20 s at 10 mm) in a chairside air-abrasion device. After ultrasonic cleaning again, universal primers were applied according to each manufacturer's recommendation. The resin cement (RelyX ARC, 3M ESPE) was built up incrementally and photo-polymerized on the zirconia surface using a silicone mold (empty set = 3.5, height = 3 mm). All specimens were stored in distilled water (60 days at 37 degrees C) and then subjected to shear bond strength testing (SBS) in a universal testing machine (1 mm/min). On a separate set of zirconia specimens, contact angle measurements were made using the sessile drop technique with a goniometer after the application of universal primers on control and air-abraded zirconia surfaces. Data (MPa) were analyzed using one-way ANOVA, Tukey's test, and Student's t-test (alpha = 0.05).Results: When universal primers were used alone, SbU presented significantly higher mean SBS (19.5 +/- 5.8) that did the other primers (0 to 9.9 +/- 6.6) (p = 0.001). When air abraded, the groups AP-A (14.1 +/- 6.1), MP-A (15.9 +/- 5.4), ZP-A (16.9 +/- 7.3), SG-A (19.1 +/- 2.1), SbU-A (12 +/- 1.5) showed significant differences (p = 0.03). Adhesive performance of all universal primers was enhanced after air abrasion, with the exception of the SbU and MZ primers. After air abrasion, contact angle measurements were lower for the each primer (without air abrasion: 28.9 to 83.9; with air abrasion: 27.1 to 63.0), except for MZP.Conclusion: Air abrasion with 110 mu m Al2O3 followed by universal primer application increased the bond strength of tested resin cement to zirconia, with the exception of SbU and MZ.en
dc.description.affiliationFed Univ Rio Grande Norte UFRN, Dept Dent, Natal, RN, Brazil
dc.description.affiliationUniv Estadual Paulista, UNESP, Inst Sci &Technol, Dept Dent Mat &Prosthodont, Sao Jose Dos Campos, Brazil
dc.description.affiliationFed Univ Paraiba UFPB, Dept Dent Mat &Prosthodont, Joao Pessoa, Paraiba, Brazil
dc.description.affiliationFed Univ Paraiba UFPB, Dept Restorat Dent, Joao Pessoa, Paraiba, Brazil
dc.description.affiliationUniv Fed Rio Grande do Norte, Div Prosthodont, Dept Restorat Dent, Natal, RN, Brazil
dc.description.affiliationUniv Zurich, Ctr Dent &Oral Med, Dent Mat Unit, Clin Fixed &Removable Prosthodont &Dent Mat Sci, Zurich, Switzerland
dc.description.affiliationUnespUniv Estadual Paulista, UNESP, Inst Sci &Technol, Dept Dent Mat &Prosthodont, Sao Jose Dos Campos, Brazil
dc.format.extent169-174
dc.identifierhttp://jad.quintessenz.de/index.php?doc=abstract&abstractID=33974
dc.identifier.citationJournal Of Adhesive Dentistry, v. 17, n. 2, p. 169-174, 2015.
dc.identifier.doi10.3290/j.jad.a33974
dc.identifier.issn1461-5185
dc.identifier.urihttp://hdl.handle.net/11449/128898
dc.identifier.wosWOS:000355986200010
dc.language.isoeng
dc.publisherQuintessence Publishing Co Inc
dc.relation.ispartofJournal Of Adhesive Dentistry
dc.relation.ispartofjcr1.691
dc.relation.ispartofsjr0,839
dc.rights.accessRightsAcesso restrito
dc.sourceWeb of Science
dc.subjectadhesionen
dc.subjectaluminum oxideen
dc.subjectshear bond strengthen
dc.subjectwettabilityen
dc.subjectyttria stabilized tetragonal zirconiaen
dc.titleCan Application of Universal Primers Alone Be a Substitute for Airborne-Particle Abrasion to Improve Adhesion of Resin Cement to Zirconia?en
dc.typeArtigo
dcterms.rightsHolderQuintessence Publishing Co Inc
dspace.entity.typePublication
unesp.campusUniversidade Estadual Paulista (UNESP), Instituto de Ciência e Tecnologia, São José dos Campospt
unesp.departmentMateriais Odontológicos e Prótese - ICTpt