Surface degradation of glass ceramics after exposure to acidulated phosphate fluoride

dc.contributor.authorCcahuana, Vanessa Zulema S. [UNESP]
dc.contributor.authorOzcan, Mutlu
dc.contributor.authorMelo Mesquita, Alfredo Mikail [UNESP]
dc.contributor.authorNishioka, Renato Sussumo [UNESP]
dc.contributor.authorKimpara, Estevão Tomomitsu [UNESP]
dc.contributor.authorBottino, Marco Antonio [UNESP]
dc.contributor.institutionUniversity of Zurich
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2014-05-20T14:05:07Z
dc.date.available2014-05-20T14:05:07Z
dc.date.issued2010-03-01
dc.description.abstractObjective: This study evaluated the surface degradation effect of acidulated phosphate fluoride (APF) gel exposure on the glassy matrix ceramics as a function of time. Material and methods: Disc-shaped ceramic specimens (N = 120, 10/per ceramic material) were prepared in stainless steel molds (inner diameter: 5 mm, height: 2 mm) using 6 dental ceramics: 3 indicated for ceramic-fused-to-metal (Vita Omega 900, Carmen and Vita Titankeramik), 2 for all-ceramic (Vitadur Alpha and Finesse (R) Low Fusing) and 1 for both types of restorations (IPS d. SIGN). The specimens were wet ground finished, ultrasonically cleaned and auto-glazed. All specimens were subjected to calculation of percentage of mass loss, surface roughness analysis and topographical description by scanning electron microscopy (SEM) before (0 min) and after exposure to 1.23 % APF gel for 4 min and 60 min representing short-and long-term etching effect, respectively. The data were analyzed using two-way ANOVA with repeated measures and Tukey` s test (alpha=0.05). Results: Significant effect of the type of the ceramics (p=0.0000, p=0.0031) and exposure time (p=0.0000) was observed in both surface roughness and percentage of mass loss values, respectively. The interaction factor between both parameters was also significant for both parameters (p=0.0904, p=0.0258). Both 4 min (0.44 +/- 0.1-0.81 +/- 0.2 mu m) and 60 min (0.66 +/- 0.1 - 1.04 +/- 0.3 mu m) APF gel exposure created significantly more surface roughness for all groups when compared to the control groups (0.33 +/- 0.2-0.68 +/- 0.2 mu m) (p<0.05). There were no significant differences in percentage of mass loss between the ceramics at 4 min (p>0.05) but at 60 min exposure, IPS d. SIGN showed the highest percentage of mass loss (0.1151 +/- 0.11). The mean surface roughness for Vita Titankeramik (0.84 +/- 0.2 mu m) and Finesse (R) Low Fusing (0.74.+/- 0.2 mu m) was significantly higher than those of the other ceramics (0.59 +/- 0.1 mu m - 0.49 +/- 0.1 mu m) and Vita Titankeramik (p<0.05) regardless of the exposure time. A positive correlation was found between surface roughness and percentage of mass loss for all ceramic materials [(r=0.518 (Vitadur Alpha), r=0.405 (Vita Omega 900), r=0.580 (Carmen), r=0.687 (IPS d. SIGN), r=0.442 (Finesse (R) Low Fusing), r=0.572 (Vita Titankeramik), Pearson's correlation coefficient)]. The qualitative SEM analysis showed evidence of corrosive attack on all of ceramics at varying degrees. Conclusions: The ceramics indicated for either metal-ceramic or all-ceramic restorations were all vulnerable to surface texture changes and mass loss after short-term and long-term APF gel exposure.en
dc.description.affiliationUniv Zurich, Head Dent Mat Unit, Ctr Dent & Oral Med, Clin Fixed & Removable Prosthodont & Dent Mat Sci, CH-8032 Zurich, Switzerland
dc.description.affiliationSão Paulo State Univ, Dept Dent Mat & Prosthodont, Sao Jose dos Campos Dent Sch, Sao Jose Dos Campos, Brazil
dc.description.affiliationUnespSão Paulo State Univ, Dept Dent Mat & Prosthodont, Sao Jose dos Campos Dent Sch, Sao Jose Dos Campos, Brazil
dc.format.extent155-165
dc.identifierhttp://dx.doi.org/10.1590/S1678-77572010000200010
dc.identifier.citationJournal of Applied Oral Science. Bauru-sp: Univ São Paulo Fac Odontologia Bauru, v. 18, n. 2, p. 155-165, 2010.
dc.identifier.fileS1678-77572010000200010.pdf
dc.identifier.issn1678-7757
dc.identifier.lattes0967916388665754
dc.identifier.lattes9234456003563666
dc.identifier.lattes0056660842284397
dc.identifier.orcid0000-0003-0586-4644
dc.identifier.orcid0000-0002-1458-601X
dc.identifier.scieloS1678-77572010000200010
dc.identifier.urihttp://hdl.handle.net/11449/22841
dc.identifier.wosWOS:000277832000010
dc.language.isoeng
dc.publisherUniversidade de São Paulo (USP), Faculdade de Odontologia de Bauru
dc.relation.ispartofJournal of Applied Oral Science
dc.relation.ispartofjcr1.709
dc.relation.ispartofsjr0,645
dc.rights.accessRightsAcesso aberto
dc.sourceWeb of Science
dc.subjectAcidulated phosphate fluorideen
dc.subjectDental ceramicsen
dc.subjectDental materialsen
dc.subjectLoss mass analysisen
dc.subjectMicroscopy, electron, scanningen
dc.subjectSurface roughnessen
dc.titleSurface degradation of glass ceramics after exposure to acidulated phosphate fluorideen
dc.typeArtigo
dcterms.licensehttp://www.scielo.br/revistas/jaos/paboutj.htm
dcterms.rightsHolderUniv São Paulo Fac Odontologia Bauru
dspace.entity.typePublication
unesp.author.lattes0967916388665754[5]
unesp.author.lattes9234456003563666
unesp.author.lattes0056660842284397[4]
unesp.author.orcid0000-0003-0586-4644[5]
unesp.author.orcid0000-0002-1458-601X[4]
unesp.campusUniversidade Estadual Paulista (UNESP), Instituto de Ciência e Tecnologia, São José dos Campospt
unesp.departmentMateriais Odontológicos e Prótese - ICTpt

Arquivos

Pacote Original

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
S1678-77572010000200010.pdf
Tamanho:
514.93 KB
Formato:
Adobe Portable Document Format
Descrição:

Licença do Pacote

Agora exibindo 1 - 2 de 2
Carregando...
Imagem de Miniatura
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição:
Carregando...
Imagem de Miniatura
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: