Publicação: Strength of 3Y-TZP and feldspathic porcelain subjected to different cooling methods
dc.contributor.author | Almeida-júnior, Antonio Alves De | |
dc.contributor.author | Longhini, Diogo | |
dc.contributor.author | Galvão, Beatriz Regalado | |
dc.contributor.author | Santos, Claudinei Dos | |
dc.contributor.author | Adabo, Gelson Luis | |
dc.contributor.institution | Universidade Tiradentes School of Dentistry Department of Oral Rehabilitation | |
dc.contributor.institution | Universidade Estadual Paulista (Unesp) | |
dc.contributor.institution | Universidade Potiguar School of Dentistry Department of Oral Rehabilitation | |
dc.contributor.institution | Universidade do Estado do Rio de Janeiro (UERJ) | |
dc.date.accessioned | 2015-02-02T12:39:28Z | |
dc.date.available | 2015-02-02T12:39:28Z | |
dc.date.issued | 2014-04-01 | |
dc.description.abstract | AIM: To investigate the effect of the cooling rate on flexural strength of monolayer and bilayer porcelain/zirconia (Y-TZP) bars. METHODS: Forty-five specimens were made for each design group: (PM) monolithic specimens of veneer porcelain Vita VM9 (Vita, Germany); (ZM) monolithic specimens of zirconia (ZiHP; ProtMat, Brazil); (PB) bilayer specimens zirconia/porcelain with porcelain on lower surface; and (ZB) bilayer specimens porcelain/zirconia with zirconia on lower surface. Each group was cooled by three different methods after porcelain sintering: slow specimens were cooled inside the turned-off furnace; normal specimens were removed from the furnace and cooled in air at room temperature; and fast specimens were removed from the furnace at 910°C and cooled by compressed air for 10 s. Specimens were polished and flexural strength was measured in water at 37 °C (n=15). Maximum load at fracture was recorded, and equations for simple (monolayer) and composite (bilayer) structures were used to calculate the flexural strength. RESULTS were analyzed using one-way ANOVA (p<0.05) and Tukey test separately for each design. RESULTS: The results of one-way ANOVA were statistically significant only for the PB group. The post-hoc Tukey test showed the highest flexural strength for fast cooling and the lowest for slow cooling; the normal cooling was statistically similar to both. CONCLUSIONS: Cooling methods affected only the flexural strength of bilayer specimens with porcelain on low surface (under tension) when the slow cooling method was used. | en |
dc.description.affiliation | Universidade Tiradentes School of Dentistry Department of Oral Rehabilitation | |
dc.description.affiliation | Universidade Estadual Paulista School of Dentistry Department of Dental Materials and Prosthodontics | |
dc.description.affiliation | Universidade Potiguar School of Dentistry Department of Oral Rehabilitation | |
dc.description.affiliation | Universidade do Estado do Rio de Janeiro Resende School of Technology Department of Engineering Materials | |
dc.description.affiliationUnesp | Universidade Estadual Paulista School of Dentistry Department of Dental Materials and Prosthodontics | |
dc.description.sponsorship | Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP) | |
dc.description.sponsorship | Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq) | |
dc.description.sponsorship | Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES) | |
dc.format.extent | 124-128 | |
dc.identifier | http://dx.doi.org/10.1590/1677-3225v13n2a09 | |
dc.identifier.citation | Brazilian Journal of Oral Sciences. Faculdade de Odontologia de Piracicaba - UNICAMP, v. 13, n. 2, p. 124-128, 2014. | |
dc.identifier.doi | 10.1590/1677-3225v13n2a09 | |
dc.identifier.file | S1677-32252014000200124.pdf | |
dc.identifier.issn | 1677-3225 | |
dc.identifier.lattes | 2851339311179809 | |
dc.identifier.scielo | S1677-32252014000200124 | |
dc.identifier.uri | http://hdl.handle.net/11449/114365 | |
dc.language.iso | eng | |
dc.publisher | Faculdade de Odontologia de Piracicaba - UNICAMP | |
dc.relation.ispartof | Brazilian Journal of Oral Sciences | |
dc.relation.ispartofsjr | 0,131 | |
dc.rights.accessRights | Acesso aberto | pt |
dc.source | SciELO | |
dc.subject | dental porcelain | en |
dc.subject | zirconium | en |
dc.subject | material resistance | en |
dc.title | Strength of 3Y-TZP and feldspathic porcelain subjected to different cooling methods | en |
dc.type | Artigo | pt |
dspace.entity.type | Publication | |
relation.isDepartmentOfPublication | 3936e2e2-946a-42ab-8b9d-9521513200fc | |
relation.isDepartmentOfPublication.latestForDiscovery | 3936e2e2-946a-42ab-8b9d-9521513200fc | |
relation.isOrgUnitOfPublication | ca4c0298-cd82-48ee-a9c8-c97704bac2b0 | |
relation.isOrgUnitOfPublication.latestForDiscovery | ca4c0298-cd82-48ee-a9c8-c97704bac2b0 | |
unesp.author.lattes | 2851339311179809 | |
unesp.author.orcid | 0000-0002-0734-7926[5] | |
unesp.campus | Universidade Estadual Paulista (UNESP), Faculdade de Odontologia, Araraquara | pt |
unesp.department | Materiais Odontológicos e Prótese - FOAR | pt |
Arquivos
Pacote Original
1 - 1 de 1
Carregando...
- Nome:
- S1677-32252014000200124.pdf
- Tamanho:
- 106.16 KB
- Formato:
- Adobe Portable Document Format