Publicação: Heat treatment-improved bond strength of resin cement to lithium disilicate dental glass-ceramic
dc.contributor.author | Sundfeld, Daniel | |
dc.contributor.author | Correr-Sobrinho, Lourenço | |
dc.contributor.author | Pini, Núbia Inocêncya Pavesi | |
dc.contributor.author | Costa, Ana Rosa | |
dc.contributor.author | Sundfeld, Renato Herman [UNESP] | |
dc.contributor.author | Pfeifer, Carmem Silvia | |
dc.contributor.author | Martins, Luis Roberto Marcondes | |
dc.contributor.institution | Universidade Estadual de Campinas (UNICAMP) | |
dc.contributor.institution | Oregon Health and Science University - OHSU | |
dc.contributor.institution | Universidade Estadual Paulista (Unesp) | |
dc.date.accessioned | 2018-12-11T17:28:56Z | |
dc.date.available | 2018-12-11T17:28:56Z | |
dc.date.issued | 2016-06-01 | |
dc.description.abstract | This study investigated the influence of different hydrofluoric acid (HF) concentrations and heat treatments applied to a lithium disilicate dental glass-ceramic (EMX) on surface morphology and micro-shear bond strength (μSBS) to resin cement. Five HF concentrations (1%, 2.5%, 5%, 7.5% and 10%) and four different heat treatments applied before etching were assessed: 1. etching at room temperature with no previous heat treatment (control group); 2. HF stored at 70 °C for 1 min applied to the ceramic surface at room temperature; 3. HF at room temperature applied after a hot air stream is applied perpendicularly to the ceramic surface for 1 min; 4. The combination of previously heated HF and heated EMX surface. The etching time was fixed for 20 s for all groups. Etched EMX specimens were analyzed on field-emission scanning electron microscope (FE-SEM) and the μSBS was carried out on a universal testing machine at a crosshead speed of 1 mm/min until fracture. For the control groups, FE-SEM images showed greater glassy matrix dissolution and higher μSBS for 7.5% and 10% HF concentrations. The previous heat treatments enhanced the glassy matrix dissolution more evidently for 1%, 2.5% and 5% and yielded increased μSBS values, which were not statistically different for 7.5% and 10% HF concentrations (control group). HF concentrations and previous heat treatments did show to have an influence on the etching/bonding characteristics to lithium disilicate dental glass-ceramic. | en |
dc.description.affiliation | Department of Restorative Dentistry Piracicaba Dental School University of Campinas UNICAMP | |
dc.description.affiliation | Department of Restorative Dentistry Division of Biomaterials and Biomechanics Oregon Health and Science University - OHSU | |
dc.description.affiliation | Department of Restorative Dentistry Dental Materials Division Piracicaba Dental School University of Campinas - UNICAMP | |
dc.description.affiliation | Department of Restorative Dentistry Araçatuba Dental School State University of São Paulo UNESP | |
dc.description.affiliationUnesp | Department of Restorative Dentistry Araçatuba Dental School State University of São Paulo UNESP | |
dc.description.sponsorship | Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP) | |
dc.format.extent | 10071-10078 | |
dc.identifier | http://dx.doi.org/10.1016/j.ceramint.2016.03.112 | |
dc.identifier.citation | Ceramics International, v. 42, n. 8, p. 10071-10078, 2016. | |
dc.identifier.doi | 10.1016/j.ceramint.2016.03.112 | |
dc.identifier.file | 2-s2.0-84977962715.pdf | |
dc.identifier.issn | 0272-8842 | |
dc.identifier.scopus | 2-s2.0-84977962715 | |
dc.identifier.uri | http://hdl.handle.net/11449/178136 | |
dc.language.iso | eng | |
dc.relation.ispartof | Ceramics International | |
dc.relation.ispartofsjr | 0,784 | |
dc.rights.accessRights | Acesso aberto | pt |
dc.source | Scopus | |
dc.subject | B. Electron microscopy | |
dc.subject | B. Surfaces | |
dc.subject | C. Strength | |
dc.subject | D. Glass ceramics | |
dc.subject | E. Biomedical applications | |
dc.title | Heat treatment-improved bond strength of resin cement to lithium disilicate dental glass-ceramic | en |
dc.type | Artigo | pt |
dspace.entity.type | Publication | |
relation.isOrgUnitOfPublication | 8b3335a4-1163-438a-a0e2-921a46e0380d | |
relation.isOrgUnitOfPublication.latestForDiscovery | 8b3335a4-1163-438a-a0e2-921a46e0380d | |
unesp.campus | Universidade Estadual Paulista (UNESP), Faculdade de Odontologia, Araçatuba | pt |
unesp.department | Odontologia Restauradora - FOA | pt |