Clinical evaluation of the failure rate of metallic brackets bonded with orthodontic composites

dc.contributor.authorRomano, Fábio Lourenço
dc.contributor.authorValério, Rodrigo Alexandre
dc.contributor.authorGomes-Silva, Jaciara Miranda
dc.contributor.authorFerreira, José Tarcísio Lima
dc.contributor.authorFaria, Gisele [UNESP]
dc.contributor.authorBorsatto, Maria Cristina
dc.contributor.institutionUniversidade de São Paulo (USP)
dc.contributor.institutionUniversidade Estadual Paulista (Unesp)
dc.date.accessioned2014-05-27T11:27:25Z
dc.date.available2014-05-27T11:27:25Z
dc.date.issued2012-12-17
dc.description.abstractThe purpose of the present study was to evaluate in vivo the failure rate of metallic brackets bonded with two orthodontic composites. Nineteen patients with ages ranging from 10.5 to 38.7 years needing corrective orthodontic treatment were selected for study. The enamel surfaces from second premolars to second premolars were treated with Transbond Plus-Self Etching Primer (3M Unitek). Next, 380 orthodontic brackets were bonded on maxillary and mandibular teeth, as follows: 190 with Transbond XT composite (3M Unitek) (control) and 190 with Transbond Plus Color Change (3M Unitek) (experimental) in contralateral quadrants. The bonded brackets were light cured for 40 s, and initial alignment archwires were inserted. Bond failure rates were recorded over a six-month period. At the end of the evaluation, six bond failures occurred, three for each composite. Kaplan-Meyer method and log-rank test (Mantel-Cox) was used for statistical analysis, and no statistically significant difference was found between the materials (p=0.999). Both Transbond XT and Transbond Plus Color Change composites had low debonding rates over the study period.en
dc.description.affiliationDepartment of Pediatric Clinics Preventive and Community Dentistry, Ribeirão Preto Dental School USP - University of São Paulo, Ribeirão Preto, SP
dc.description.affiliationDepartment of Restorative Dentistry Araraquara Dental School Universidade Estadual Paulista (UNESP), Araraquara, SP
dc.description.affiliationUnespDepartment of Restorative Dentistry Araraquara Dental School Universidade Estadual Paulista (UNESP), Araraquara, SP
dc.format.extent399-402
dc.identifierhttp://dx.doi.org/10.1590/S0103-64402012000400015
dc.identifier.citationBrazilian Dental Journal, v. 23, n. 4, p. 399-402, 2012.
dc.identifier.doi10.1590/S0103-64402012000400015
dc.identifier.file2-s2.0-84870941590.pdf
dc.identifier.issn0103-6440
dc.identifier.issn1806-4760
dc.identifier.lattes1411074363039082
dc.identifier.scieloS0103-64402012000400015
dc.identifier.scopus2-s2.0-84870941590
dc.identifier.urihttp://hdl.handle.net/11449/74074
dc.language.isoeng
dc.relation.ispartofBrazilian Dental Journal
dc.relation.ispartofsjr0,476
dc.rights.accessRightsAcesso aberto
dc.sourceScopus
dc.subjectDebonding
dc.subjectOrthodontic brackets
dc.subjectOrthodontics
dc.titleClinical evaluation of the failure rate of metallic brackets bonded with orthodontic compositesen
dc.typeArtigo
dcterms.licensehttp://www.scielo.br/revistas/bdj/iaboutj.htm
dspace.entity.typePublication
unesp.author.lattes1411074363039082
unesp.campusUniversidade Estadual Paulista (UNESP), Faculdade de Odontologia, Araraquarapt
unesp.departmentOdontologia Restauradora - FOARpt

Arquivos

Pacote Original

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
2-s2.0-84870941590.pdf
Tamanho:
400.92 KB
Formato:
Adobe Portable Document Format